Mitigate reflow issues in PCB assembly processes.

To prevent PCB bending and warping during reflow, consider lowering furnace temperature, using high Tg PCBs, increasing board thickness, reducing board size and panel number, using furnace trays, and opting for routing over V-Cut for sub-boards.

Mitigate reflow issues in PCB assembly processes. Read More »