Production of FR4 PCBs faces significant challenges due to extreme heat conditions
The potential bursting of FR4 PCBs during back welding is a result of the high heat stress and thermal expansion differences, especially in areas with dense through-holes and large surface copper areas, making it important to carefully manage the reflow process and consider alternatives to reduce the risk.
Production of FR4 PCBs faces significant challenges due to extreme heat conditions Read More »