Identifying Causes of PCB Insulating Paint Peeling Post-Tin Furnace

Peeling of green paint on circuit boards may result from inadequate durability of the paint, external factors like flux or mechanical impacts, or moisture absorption, while S/M peeling after chemical nickel gold could stem from improper copper processing, insufficient drying of coatings, oxide layer stagnation, unsuitable paint for gold ranges, poor polymerization, or excessive high-temperature processes, necessitating thorough analysis and proper handling techniques for optimal production.